| ISO | Material | Condition | Tensile strength [N/mm2] | Hardness HB | AH725 Cutting speed (m/min) | |
| < 0.25 %C | Annealed | 420 | 125 | 100-250 | ||
| Non-alloy steel and | ≥ 0.25 %C | Annealed | 650 | 190 | 80-210 | |
| cast steel, free cutting | < 0.55 %C | Quenched and tempered | 850 | 250 | 65-170 | |
| steel | ≥ 0.55 %C | Annealed | 750 | 220 | 110-180 | |
| Quenched and tempered | 1000 | 300 | 95-160 | |||
| Annealed | 600 | 200 | 90-160 | |||
| Low alloy steel and cast | steel | 930 | 275 | 65-200 | ||
| (less than 5% of alloying | elements) | Quenched and tempered | 1000 | 300 | 70-210 | |
| 1200 | 350 | 95-160 | ||||
| High alloyed steel, cast s | teel, | Annealed | 680 | 200 | 130-170 | |
| and tool steel | Quenched and tempered | 1100 | 325 | 75-100 | ||
| Stainless steel and cast | teel | Ferritic/martensitic | 680 | 200 | 110-170 | |
| Martensitic | 820 | 240 | 70-155 | |||
| Stainless steel | Annealed | 600 | 180 | 85-100 | ||
| Cast iron nodular (GGG) | Ferritic/martensitic | 180 | 120-160 | |||
| Pearlitic | 260 | 75-160 | ||||
| Grey cast iron (GG) | Ferritic | 160 | 70-150 | |||
| Pearlitic | 250 | 110-140 | ||||
| Mllbl t i | Ferritic | 130 | 120-160 | |||
| aeae cas ron | Pearlitic | 230 | 110-140 | |||
| Not cureable | 60 | 160-300 | ||||
| Aluminum- wrought alloy | Cured | 100 | ||||
| ≤12% Si | Not cureable | 75 | 150-350 | |||
| Aluminum-cast, alloyed | Cured | 90 | ||||
| >12% Si | High temperature | 130 | 100-250 | |||
| >1% Pb | Free cutting | 110 | ||||
| Copper alloys | Brass | 90 | ||||
| Electrolitic copper | 100 | |||||
| Non-metallic | Duroplastics, fiber plastics | 100-400 | ||||
| Hard rubber | ||||||
| F bd | Annealed | 200 | ||||
| e ase | Cured | 280 | ||||
| High temp. alloys | Annealed | 250 | 20-80 | |||
| Ni or Co based | Cured | 350 | ||||
| Cast | 320 | |||||
| Titi Ti ll | RM 400 | |||||
| anum aoys | Alpha+beta alloys cured | RM 1050 | 20-80 | |||
| Hardened steel | Hardened | 55 HRC | 55-65 | |||
| Hardened | 60 HRC | 45-55 | ||||
| Chilled cast iron | Cast | 400 | 90-105 | |||
| Cast iron | Hardened | 55 HRC | 55-65 |