GAMP = 0°, GAMF = -14°GAMP = 0°, GAMF = -14°
LF R
A R R C
| 4°(KAPR) | A | A-A cross sectionA - A | |
| 断面 |
| Designation DC | CICT | OAL | LF | H | DCSFMS | CRKS | WT(kg) | Air hole | Insert | ||
| HFWX04M016M08R02 | 16 | 2 | 42 | 25 | 10 | 13 | M8 | 0.03 | With | WXHU04... | D |
| HFWX04M020M10R03 | 20 | 3 | 49 | 30 | 15 | 18 | M10 | 0.05 | With | WXHU04... | |
| HFWX04M025M12R04 | 25 | 4 | 52 | 30 | 17 | 21 | M12 | 0.09 | With | WXHU04... | |
| Please see the page H210 for TungFlex modular shank. | |||||||||||
| SPARE PARTS | E |
| Designation | Clamping screw | Lubricant | Wrench | |
| HFWX04M... | SR34-514 | M-1000 | T-7F |
*Recommended clamping torque (N·m) :SR34-514=0.9 INSERT F W X H U - M J S
| P | Steel | H | |
| M | Stainless | ||
| K | Cast iron | ||
| N | Non-ferrous | ||
| S | Superalloys | : First choice | |
| Hard materials | : Second choice | ||
| H | |||
| Coated | I |
| Designation | RE | APMX | IC | S | |||
| WXHU040305R-MJ | 0.5 | 0.5 | z | 6.35 | 3.18 | ||
| WXHU040310R-MJ | 1 | 1 | z | 6.35 | 3.18 | J |
* For plunging, the maximum cutting width is 2 mm. z: Line up STANDARD CUTTING CONDITIONS
| ISO | Workpiece material | Hardness | Grade | Cutting speed Vc (m/min) | Feed per tooth fz (mm/t) |
| High carbon steel S45C, S55C, etc. C45, C55, etc. Alloy steel SCM440, etc. 42CrMo4, SCr145, etc. | 200 - 300 HB 150 - 300 HB | AH110 AH110 | 100 - 300 100 - 300 | 0.1 - 0.3 0.1 - 0.3 | |
| Prehardened steel NAK80, PX5, etc. | 30 - 40 HRC | AH110 | 100 - 300 | 0.05 - 0.3 | |
| Hardened steel SKD61, etc. X40CrMoV5-1, etc. | 40 - 50 HRC | AH110 | 80 - 130 | 0.1 - 0.3 | |
| SKD11, etc. X153CrMoV12, etc. | 50 - 60 HRC | AH110 | 50 - 100 | 0.05 - 0.15 |
Hardened steel M