LNXT
A recommended cutting conditions | A
Complementos | Repuestos Condições de corte recomendadas | Condiciones de corte recomendables Vc (m/min) HB Feed fz (mm/t)
Order separately Order separately ISO PSM Material Wear Resistance Toughness
Key (Brinell)
Insert Screw Key (Torx) (Torx - Nm) Torque Value Screw DIN 6368 Wrench PH5320 PH7920 PHS740 PH7740 LNXT 13… MP
Cutter
ØDc 1 Unalloyed Steel 125-220 - 180-250 140-170 140-170 0,10-0,35
Nm Nm
| P | 2 | Low-Alloyed Steel | 220-280 | - | 170-210 | 130-160 | 130-160 | 0,10-0,30 | |||||||||||||
| E90190 - 25 | P0400900 | XT15 | DT1530 | 3,0 | - | - | 3 | High-Alloyed Steel | 280-380 | - | 160-200 | 110-140 | 110-140 | 0,10-0,20 | |||||||
| E90190 - 32-40 | P0401200 | XT15 | DT1530 | 3,0 | - | - | 4 | SS - Ferritic / Martensitic | 200-330 | - | - | - | 120-180 | 0,10-0,30 | |||||||
| W90190 - 25 | P0400900 | XT15 | DT1530 | 3,0 | - | - | M | 5 | SS - Austenitic | 200-330 | - | - | - | 100-150 | 0,10-0,25 | ||||||
| W90190 - 32-40 | P0401200 | XT15 | DT1530 | 3,0 | - | - | 6 | SS - Austenitic-ferritic (Duplex) | 230-260 | - | - | - | 70-130 | 0,10-0,20 | |||||||
| A90190 - 40-63 | P0401200 | XT15 | DT1530 | 3,0 | - | - | 7 | Malleable Cast Iron | 130-230 | 180-320 | 170-300 | - | - | 0,10-0,35 | |||||||
| A90190 - 80 | P0401200 | XT15 | DT1530 | 3,0 | J0123510 | SD6368-12 | K | 8 | Grey Cast Iron | 180-245 | 160-270 | 150-250 | - | - | 0,10-0,30 | ||||||
| A90190 - 100 | P0401200 | XT15 | DT1530 | 3,0 | J0164110 | SD6368-16 | 9 | Nodular Cast iron | 160-250 | 100-230 | 90-210 | - | - | 0,10-0,25 | |||||||
| A90190 -125 | P0401200 | XT15 | DT1530 | 3,0 | J0204610 | SD6368-20 | (Note 1) Cutting conditions ae/Dc=70%. |
Note: The toolholder is supplied with the XT/PT key. To order the DT key please check the page A-243. (Note 2) It’s possible to occur vibrations in certain cases. Please reduce depth of cut and / or reduce cutting conditions in following cases: Check the procedures for the clamping screws on the page A-243. - When using long shank; - When using long tool overhang with arbor type; - When application has poor clamping rigidity or when using a low rigidity machine.
Guia para selecção de graus | Tabla para selección de calidades Grades HB Wear Resistance Toughness
ISO PSM Material (Brinell)
PH5320 PH7920 PHS740 PH7740
| 1 | Unalloyed Steel | 125-220 | ✓ | ✓ | ✓ | |||
| P | 2 | Low-Alloyed Steel | 220-280 | ✓ | ✓ | ✓ | ||
| 3 | High-Alloyed Steel | 280-380 | ✓ | ✓ | ✓ | |||
| 4 | SS - Ferritic / Martensitic | 200-330 | ✓ | |||||
| M | 5 | SS - Austenitic | 200-330 | ✓ | ||||
| 6 | SS - Austenitic-ferritic (Duplex) | 230-260 | ✓ | |||||
| 7 | Malleable Cast Iron | 130-230 | ✓ | ✓ | ✓ | Good Conditions | ||
| K | 8 | Grey Cast Iron | 180-245 | ✓ | ✓ | ✓ | Average Conditions | |
| 9 | Nodular Cast iron | 160-250 | ✓ | ✓ | ✓ | Difficult Conditions |