SEHT | SEHW
A recommended cutting conditions | WIPER INSERTS A
Condições de corte recomendadas | Condiciones de corte recomendables
| ISO | PSM | Material | HB (Brinell) | Wear Res PH0910 | Vc (m/min) istanceT PH6920 | oughness PH6740 | SEHT 13T3 AGSN | Feed fz SEHW 13T3 AGFN | (mm/t) SEHT 13T3 AGFN-LN | SEHT 13T3 AGSN-W |
| 1 | Unalloyed Steel | 125-220 | - | 150-230 | 130-160 | 0,10-0,25 | - | - | 0,10-0,30 | |
| P | 2 | Low-Alloyed Steel | 220-280 | - | 140-220 | 120-150 | 0,10-0,20 | - | - | 0,10-0,30 |
| 3 | High-Alloyed Steel | 280-380 | - | 130-180 | 100-130 | 0,10-0,20 | - | - | 0,10-0,30 | |
| 4 | SS - Ferritic / Martensitic | 200-330 | - | - | 100-120 | 0,10-0,20 | - | - | - | |
| M | 5 | SS - Austenitic | 200-330 | - | - | 80-110 | 0,10-0,20 | - | - | - |
| 6 | SS - Austenitic-ferritic (Duplex) | 230-260 | - | - | 70-100 | 0,10-0,20 | - | - | - | |
| 7 | Malleable Cast Iron | 130-230 | - | 150-280 | 130-250 | 0,10-0,25 | 0,10-0,25 | - | 0,10-0,30 | |
| K | 8 | Grey Cast Iron | 180-245 | 130-230 | 110-220 | 0,10-0,25 | 0,10-0,25 | - | 0,10-0,30 | |
| 9 | Nodular Cast iron | 160-250 | 80-190 | 80-170 | 0,10-0,20 | 0,10-0,20 | - | 0,10-0,30 | ||
| N | 10 | Aluminium and Non Ferrous | 30-130 | 350-1400 | - | - | - | - | 0,10-0,20 | - |
- The width of parallel land (F) of the SEHT insert is 2,0 mm. - To obtain a good surface finishing, the feed per revolution should be a maximum 80% of 2,0 mm = 1,6 mm. - Result: Feed per revolution (fn) could be increased from 1,6 mm to 60% of 6,0 mm = 4,9 mm.
(Note 1) Cutting conditions ae/DC=70% (Note 2) Cutting conditions should be ajusted according to the machine and work rigidity. (Note 3) If chattering occurs, reduce ap and Vc by 30% and keep the same fz per thooth
Guia para aplicações do quebra-aparas | Guía para aplicación del rompevirutas
When using wiper insert, install the insert as shown on Fig. A. If the insert is installed as shown on Fig. B breakage of the insert is inevitable and normal surface finish can not been obtained.
| ISO | PSM | Material | HB (Brinell) | Chip-Breaker 1st choise | Application Dificult Operations |
| 1 | Unalloyed Steel | 125-220 | SEHT... AGSN | - | |
| P | 2 | Low-Alloyed Steel | 220-280 | SEHT... AGSN | - |
| 3 | High-Alloyed Steel | 280-380 | SEHT... AGSN | - | |
| 4 | SS - Ferritic / Martensitic | 200-330 | SEHT... AGSN | SEHW... AGFN | |
| M | 5 | SS - Austenitic | 200-330 | SEHT... AGSN | SEHW... AGFN |
| 6 | SS - Austenitic-ferritic (Duplex) | 230-260 | SEHT... AGSN | SEHW... AGFN | |
| 7 | Malleable Cast Iron | 130-230 | SEHW... AGFN | - | |
| K | 8 | Grey Cast Iron | 180-245 | SEHW... AGFN | - |
| 9 | Nodular Cast iron | 160-250 | SEHW... AGFN | - | |
| N | 10 | Aluminium and Non Ferrous | 30-130 | SEHT... AGFN-LN | - |