■ In aluminum die casting and aluminum casting <2D tapping, ALS-SP solves such problems as chip jamming, chip clogging, and torn threads. Nitride
| Brass | Brass castings | Bronze | Wrought aluminum | Aluminum alloy castings | Magnesium alloy die castings | Zinc alloy castings | ||
| 10黄銅25 | 10黄銅鋳物25 | 10青銅25 | 10アルミ圧延材25 | 10アルミ合金鋳物25 | 10マグネシウム合金鋳物25 | 10亜鉛合金鋳物25 | ||
| (m/min) | (m/min) | ( m/ min) | (m/min) | (m/min) | ( m/ min) | (m/min) |
TYPE:1 TYPE:2
Segment:1D
| Size | Class | Code | Chamfer | L (inch) | ℓ (inch) | ℓn (inch) | ℓs (inch) | Ds (inch) | K (inch) | ℓk (inch) | No. of flutes | TYPE |
| For M | etric Thr | eads | l | |||||||||
| M3×0.5 | D3 | 386428M | 2.5P | 2.205 | 0.433 | 0.736 | 1.339 | 0.141 | 0.11 | 0.187 | 3 | 2 |
| M3.5×0.6 | D4 | 386429M | 2.5P | 2.205 | 0.433 | 0.748 | 1.339 | 0.141 | 0.11 | 0.187 | 3 | 2 |
| M4×0.7 | D4 | 386430M | 2.5P | 2.48 | 0.512 | 0.815 | 1.535 | 0.168 | 0.131 | 0.25 | 3 | 2 |
| M5×0.8 | D4 | 386431M | 2.5P | 2.756 | 0.551 | 0.984 | 1.654 | 0.194 | 0.152 | 0.25 | 3 | 2 |
| M6×1 | D5 | 386432M | 2.5P | 3.15 | 0.591 | 1.181 | 1.713 | 0.255 | 0.191 | 0.312 | 3 | 2 |
| M7×1 | D5 | 386433M | 2.5P | 3.543 | 0.748 | 1.339 | 1.831 | 0.318 | 0.238 | 0.375 | 3 | 3 |
| M8×1.25 | D5 | 386435M | 2.5P | 3.543 | 0.748 | 1.378 | 1.831 | 0.318 | 0.238 | 0.375 | 3 | 3 |
| M8×1 | D5 | 386434M | 2.5P | 3.543 | 0.748 | 1.378 | 1.831 | 0.318 | 0.238 | 0.375 | 3 | 3 |
| M10×1.5 | D6 | 386437M | 2.5P | 3.937 | 0.906 | 1.535 | 2.126 | 0.381 | 0.286 | 0.437 | 3 | 3 |
| M10×1.25 | D5 | 386436M | 2.5P | 3.937 | 0.906 | 1.535 | 2.126 | 0.381 | 0.286 | 0.437 | 3 | 3 |
| M12×1.75 | D6 | 386440M | 2.5P | 4.331 | 1.024 | - | 2.205 | 0.367 | 0.275 | 0.437 | 3 | 4 |
| M12×1.5 | D5 | 386439M | 2.5P | 4.331 | 1.024 | - | 2.205 | 0.367 | 0.275 | 0.437 | 3 | 4 |
| M12×1.25 | D5 | 386438M | 2.5P | 4.331 | 1.024 | - | 2.205 | 0.367 | 0.275 | 0.437 | 3 | 4 |