| Обрабатываемый | d | V | f | Обрабатываемый | d | V | f |
| 1 | c | z | 1 | c | z |
| материал | (mm) | (m/min) | (mm/z) | материал | (mm) | (m/min) | (mm/z) |
| ≤3.00 | 105 | 0.010 | ≤3.00 | 160 | 0.010 | ||
| 4.00 | 105 | 0.015 | 4.00 | 160 | 0.015 | ||
| 5.00 | 105 | 0.020 | 5.00 | 160 | 0.020 | ||
| 6.00 | 105 | 0.024 | 6.00 | 160 | 0.024 |
Сталь
8.00 105 0.032 Сталь 8.00 160 0.032
HRC<25
| 10.00 | 105 | 0.038 | HRC<25 10.00 | 160 | 0.038 |
| 12.00 | 105 | 0.046 | 12.00 | 160 | 0.046 |
| 16.00 | 105 | 0.054 | 16.00 | 160 | 0.054 |
| P 20.00 | 105 | 0.066 | P 20.00 | 160 | 0.066 |
| ≤3.00 | 75 | 0.010 | ≤3.00 | 110 | 0.010 |
| 4.00 | 75 | 0.015 | 4.00 | 110 | 0.015 |
| 5.00 | 75 | 0.020 | 5.00 | 110 | 0.020 |
| 6.00 | 75 | 0.024 | 6.00 | 110 | 0.024 |
Сталь
8.00 75 0.032 Сталь 8.00 110 0.032
HRC=25-38
| 10.00 | 75 | 0.038 | HRC=25-38 10.00 | 110 | 0.038 |
| 12.00 | 75 | 0.046 | 12.00 | 110 | 0.046 |
| 16.00 | 75 | 0.054 | 16.00 | 110 | 0.054 |
| 20.00 | 75 | 0.066 | 20.00 | 110 | 0.066 |
| ≤3.00 | 40 | 0.010 | ≤3.00 | 70 | 0.010 |
| 4.00 | 40 | 0.010 | 4.00 | 70 | 0.010 |
| Сталь HRC=45, 5.00 | 40 | 0.014 | 5.00 | 70 | 0.014 |
Сталь HRC=45,
нержавеющие 6.00 40 0.017 6.00 70 0.017
нержавеющие
M стали, 8.00 40 0.024 M 8.00 70 0.024
стали титановые
10.00 40 0.030 10.00 70 0.030
сплавы
| 12.00 | 40 | 0.036 | 12.00 | 70 | 0.036 |
| 16.00 | 40 | 0.045 | 16.00 | 70 | 0.045 |
| 20.00 | 40 | 0.057 | 20.00 | 70 | 0.057 |
| ≤3.00 | 120 | 0.010 | ≤3.00 | 130 | 0.010 |
| 4.00 | 120 | 0.015 | 4.00 | 130 | 0.015 |
| 5.00 | 120 | 0.020 | 5.00 | 130 | 0.020 |
| 6.00 | 120 | 0.024 | 6.00 | 130 | 0.024 |
Чугун,
K 8.00 120 0.032 K 8.00 130 0.032
серый чугун Чугун,
10.00 120 0.038 10.00 130 0.038
серый чугун
| 12.00 | 120 | 0.046 | 12.00 | 130 | 0.046 |
| 16.00 | 120 | 0.054 | 16.00 | 130 | 0.054 |
| 20.00 | 120 | 0.066 | 20.00 | 130 | 0.066 |
| ≤3.00 | 220 | 0.010 | ≤3.00 | 50 | 0.010 |
| 4.00 | 220 | 0.015 | 4.00 | 50 | 0.015 |
| 5.00 | 220 | 0.020 | 5.00 | 50 | 0.020 |
| Алюминиевые 6.00 | 220 | 0.024 | 6.00 | 50 | 0.024 |
| сплавы 8.00 | 220 | 0.032 | Титановые 8.00 | 50 | 0.032 |
| Si<=10% 10.00 | 220 | 0.038 | сплавы 10.00 | 50 | 0.038 |
| 12.00 | 220 | 0.046 | 12.00 | 50 | 0.046 |
| 16.00 | 220 | 0.054 | 16.00 | 50 | 0.054 |
| N 20.00 | 220 | 0.066 | H 20.00 | 50 | 0.066 |
| ≤3.00 | 90 | 0.010 | ≤3.00 | 40 | 0.010 |
| 4.00 | 90 | 0.015 | 4.00 | 40 | 0.015 |
| 5.00 | 90 | 0.020 | Сталь HRC=55, 5.00 | 40 | 0.020 |
| 6.00 | 90 | 0.024 | высокотемпера- 6.00 | 40 | 0.024 |
Латунь,
8.00 90 0.032 турные 8.00 40 0.032
бронза
| 10.00 | 90 | 0.038 | сплавы никеля | 10.00 | 40 | 0.038 |
| 12.00 | 90 | 0.046 | 12.00 | 40 | 0.046 | |
| 16.00 | 90 | 0.054 | 16.00 | 40 | 0.054 | |
| 20.00 | 90 | 0.066 | 20.00 | 40 | 0.066 |
В начале обработки рекомендуется сделать пробный проход при 85% V и 75% f относительно значений, указанных c z в таблице, с постепенным увеличением скорости подачи до рекомендованных значений при устойчивой работе. Рекомендуется использовать динамически сбалансированные зажимные патроны высокой точности и жесткости. Если биение инструмента превышает 0,01 mm, рекомендуется произвести переналадку перед возобновлением обработки.