A300 - CFRP/GFRP ∙ Roughing ∙ 8~17F

.For CFRP/GFRP rough milling. .Right helix and left helix design. .NDLC - Nano DLC coating provides exceptional wear resistance and good tool life. .DIA - Diamond coating provides exceptional wear resistance and good tool life.

Order No.Dia. (d)CL (L1)OAL (L) Shank (D)Flutes (F)
NDLCNano DLC coating
ECSSR804000L41260 68
ECSSR106000L61860 611
ECSSR408000L82460 814
ECSSR610000L103075 1016
ECSSR712000L1236100 1217
DIA Diamond Coating
ECSSR804000D41260 68
ECSSR106000D61860 611
ECSSR408000D82460 814
ECSSR610000D103075 1016
ECSSR712000D1236100 1217

ECSSR

PMKNSH

d

L1

L

D (h6)

Cutting conditions Table 073

d Tolerance
d ≤ 6 0 ~ -0.02
6 < d ≤ 12 0 ~ -0.03
d > 12 0 ~ -0.04