| Tensile | M | M-TS | MM-G | RIT K-T | YPE | MM-G | RIT P-TY | PE | |||||
| ISO Material | Condition | Strength [N/mm2] | Hardness HB | Group No. | Speed V m/min | F Fz (min) | ee Fz (max) | Speed V m/min | Feed Fz (min) | mm/t Fz (max) | Speed V m/min | Feed Fz (min) | mm/t Fz (max) |
| < 0.25 %C | Annealed | 420 | 125 | 1 | 110-140 | 0.08 | 0.20 | 110-160 | 0.05 | 0.15 | - | - | - |
| Non-alloy >= 0.25 %C | Annealed | 650 | 190 | 2 | 100-120 | 0.08 | 0.18 | 100-150 | 0.05 | 0.15 | - | - | - |
| steel and cast tl f < 0.55 %C | Quenched and tempered | 850 | 250 | 3 | 70-100 | 0.08 | 0.15 | 80-100 | 0.05 | 0.15 | - | - | - |
| see, ree cutting steel >= 0.55 %C | Annealed | 750 | 220 | 4 | 70-100 | 0.08 | 0.15 | 80-100 | 0.05 | 0.15 | - | - | - |
| Quenched and tempered | 1000 | 300 | 5 | 60-80 | 0.08 | 0.15 | 60-80 | 0.05 | 0.15 | - | - | - | |
| Annealed | 600 | 200 | 6 | 100-120 | 0.08 | 0.15 | 110-150 | 0.05 | 0.15 | - | - | - | |
| P Low alloy and cast l l h 5% f | 930 | 275 | 7 | 90-120 | 0.08 | 0.15 | 100-120 | 0.05 | 0.15 | - | - | - | |
| stee (ess tan o alloin elements) | Quenched d td | 1000 | 300 | 8 | 80-110 | 0.08 | 0.15 | 70-110 | 0.05 | 0.15 | - | - | - |
| yg | an empere | 1200 | 350 | 9 | 70-100 | 0.05 | 0.12 | 70-100 | 0.05 | 0.15 | - | - | - |
| High alloyed steel cast | Annealed | 680 | 200 | 10 | 60-80 | 0.05 | 0.18 | 60-80 | 0.05 | 0.15 | - | - | - |
| , steel and tool steel | Quenched and tempered | 1100 | 325 | 11 | 55-70 | 0.08 | 0.15 | 55-70 | 0.05 | 0.15 | - | - | - |
| Stainless steel | Ferritic/ martensitic | 680 | 200 | 12 | 100-130 | 0.06 | 0.12 | 100-130 | 0.03 | 0.15 | 100-130 | 0.03 | 0.10 |
| and cast steel | Martensitic | 820 | 240 | 13 | 100-120 | 0.08 | 0.15 | 100-130 | 0.03 | 0.15 | 100-130 | 0.03 | 0.10 |
| M Stainless steel | Austenitic | 600 | 180 | 14 | 80-120 | 0.05 | 0.10 | 90-120 | 0.03 | 0.12 | 90-120 | 0.03 | 0.10 |
| Grey cast iron (GG) | Ferritic/ pearlitic | 180 | 15 | 160-220 | 0.10 | 0.20 | 160-220 | 0.03 | 0.12 | - | - | - | |
| Pearlitic | 260 | 16 | 120-200 | 0.10 | 0.15 | 120-200 | 0.03 | 0.12 | - | - | - | ||
| K Cast iron nodular (GGG) | Ferritic | 160 | 17 | 100-140 | 0.10 | 0.20 | - | - | - | - | - | - | |
| Pearlitic | 250 | 18 | 80-100 | 0.10 | 0.15 | - | - | - | - | - | - | ||
| Ferritic | 130 | 19 | 180-250 | 0.10 | 0.20 | 180-250 | 0.03 | 0.15 | - | - | - | ||
| Malleable cast iron | Pearlitic | 230 | 20 | 160-220 | 0.10 | 0.15 | 160-220 | 0.03 | 0.15 | - | - | - | |
| Not cureable | 60 | 21 | 800-1200 | 0.10 | 0.20 | - | - | - | 800-1200 | 0.05 | 0.15 | ||
| Aluminum-wrought alloy | Cured | 100 | 22 | 800-1200 | 0.10 | 0.20 | - | - | - | 800-1200 | 0.05 | 0.15 | |
| Not cureable | 75 | 23 | - | - | - | - | - | - | 600-1000 | 0.05 | 0.15 | ||
| Aluminum- | Cured | 90 | 24 | - | - | - | - | - | - | 500-1000 | 0.05 | 0.15 | |
| cast alloys >12% Si | High | 130 | 25 | - | - | - | - | - | - | 200-400 | 0.05 | 0.15 | |
| temperature | |||||||||||||
| N >1% Pb | Free cutting | 110 | 26 | - | - | - | - | - | - | - | - | - | |
| Copper alloys | Brass | 90 | 27 | - | - | - | - | - | - | - | - | - | |
| Electrolitic copper | 100 | 28 | - | - | - | - | - | - | - | - | - | ||
| Duroplastics, | 29 | - | - | - | - | - | - | - | - | - | |||
| Non-metallic | fiberplastics | ||||||||||||
| Hard rubber | 30 | - | - | - | - | - | - | - | - | - | |||
| Fe based | Annealed | 200 | 31 | - | - | - | 30-40 | 0.02 | 0.12 | - | - | - | |
| Cured | 280 | 32 | 25-35 | 0.05 | 0.12 | 25-40 | 0.02 | 0.12 | - | - | - | ||
| High temp. | Annealed | 250 | 33 | 25-35 | 0.05 | 0.12 | 25-40 | - | - | - | 0.01 | 0.12 | |
| alloys Ni or Co | Cured | 350 | 34 | 25-35 | 0.05 | 0.12 | 25-40 | - | - | - | 0.01 | 0.12 | |
| S based | Cast | 320 | 35 | 40-60 | 0.05 | 0.12 | 25-40 | - | - | - | 0.01 | 0.12 | |
| RM 400 | 36 | 40-60 | 0.05 | 0.12 | 40-60 | - | - | - | 0.05 | 0.12 | |||
| Titanium Ti alloys | Alpha+beta | RM 1050 | 37 | 40-60 | 005 | 010 | 40-60 | - | - | - | 005 | 010 | |
| alloys cured | . | . | . | . | |||||||||
| Hardened steel | Hardened | 55 HRC | 38 | ||||||||||
| Hardened | 60 HRC | 39 | |||||||||||
| H Chilled cast iron | Cast | 400 | 40 | ||||||||||
| Cast iron | Hardened | 55 HRC | 41 |