Tensile strength [N/mm2] AM5110 AM5120 AM5120+ AM5130 AM5220 AP2025 AP2030 AP2035 AP2110 AP2120 AP2135 Recommended Cutting Data Turning – Carbide coated Cutting speed Vc [m/min] ISO Material ca. 0,15% C 350 220 - 350 220 - 320 180 - 280 170 - 240 180 - 280 190 - 240 190 - 240 180 - 230 300 - 400 250 - 350 180 - 270 Unalloyed steel and cast steel ca. 0,45% C 650 180 - 310 180 - 290 160 - 250 160 - 220 160 - 250 170 - 200 170 - 200 170 - 190 260 - 350 210 - 300 170 - 230 ca. 0,75% C 1000 150 - 270 150 - 250 120 - 220 140 - 200 120 - 220 130 - 160 130 - 160 130 - 150 240 - 300 180 - 230 160 - 210 600 180 - 300 180 - 260 - 170 - 220 160 - 250 170 - 200 170 - 200 170 - 190 220 - 300 180 - 270 160 - 220 P Low alloyed steel and cast steel 900 170 - 270 150 - 220 - 170 - 200 140 - 230 100 - 160 100 - 160 90 - 150 180 - 260 160 - 220 140 - 1801200150 - 24080 - 190-150 - 200120 - 20080 - 14080 - 14070 - 130120 - 220100 - 200100 - 160 High alloyed steel, high alloyed annealed 700 80 - 180 80 - 150 - 80 - 150 70 - 150 130 - 170 130 - 170 120 - 200 150 - 220 130 - 200 130 - 180 tool steel and cast steel hardened and tempered 1100 40 - 140 40 - 130 - 40 - 120 35 - 120 80 - 130 80 - 130 50 - 100 70 - 150 70 - 140 70 - 120 ferritic / martensitic, annealed 700 40 - 180 40 - 150 50 - 160 40 - 160 50 - 160 130 - 180 130 - 180 140 - 180 - - - Stainless steel and cast steel martensitic, hardened and tempered 1000 40 - 160 40 - 140 40 - 140 40 - 160 40 - 140 110 - 160 110 - 160 110 - 160 - - - M Stainless steel and cast steel austenitic and austenitic/ferriticchilled 450 - 600 80 - 180 80 - 160 70 - 150 80 - 150 70 - 150 100 - 170 100 - 170 110 - 190 - - -600 - 90040 - 14040 - 13035 - 12040 - 12035 - 120--80 - 150--- pearlitic, ferritic 500 - 700 180 - 350 180 - 300 180 - 300 180 - 240 180 - 300 130 - 200 130 - 200 - 160 - 230 - - Cast iron pearlitic, martensitic 700 - 850 160 - 300 160 - 280 160 - 280 160 - 220 160 - 280 120 - 180 120 - 180 - 150 - 200 - - 800 - 1100 120 - 270 120 - 240 120 - 240 120 - 200 120 - 240 - - - - - - K Cast iron with nodular graphite ferritic 550 140 - 230 140 - 230 - 140 - 200 140 - 230 120 - 170 120 - 170 - 160 - 210 - - pearlitic 800 120 - 170 120 - 170 - 110 - 160 120 - 170 120 - 190 120 - 190 - 130 - 170 - - ferritic 450 150 - 210 150 - 210 - 130 - 190 150 - 210 150 - 230 150 - 230 - 150 - 210 - - Malleable cast iron pearlitic 750 150 - 210 150 - 210 - 130 - 190 150 - 210 120 - 170 120 - 170 - 150 - 210 - - not heat treatable 200 - - - - - - - - - - - Aluminum alloys, long chipping heat treatable, heat treated 350 - - - - - - - - - - - ≤ 12% Si, hardened 250 - - - - - - - - - - - Casted aluminum alloys ≤ 12% Si, heat treatable, heat treated 300 - - - - - - - - - - - ≤ 12% Si, not heat treatable 450 - - - - - - - - - - - N Copper and copper alloys Lead alloys, Pb > 1%Brass, bronze 400 200 - 650 200 - 500 150 - 500 200 - 500 - - - - - - -300200 - 650200 - 500150 - 500200 - 500------- (brass / bronze) Aluminum bronze 500 160 - 350 160 - 300 120 - 400 150 - 220 - - - - - - - Copper and electrolyte copper 200 120 - 220 120 - 200 120 - 250 120 - 220 - - - - - - - Duroplastics 160 - 600 160 - 600 - 140 - 500 - - - - - - - Non-ferrous materials Reinforced plastics 100 - 300 100 - 300 100 - 300 100 - 300 - - - - - - - Hard rubber - - - - - - - - - - - Fe-alloyed annealed 700 20 - 70 20 - 60 20 - 60 20 - 50 20 - 60 20 - 40 - 20 - 40 - - - Fe-alloyed hardened 950 20 - 70 20 - 60 20 - 60 20 - 50 20 - 60 15 - 35 - 15 - 35 - - - High temperature resistant alloys Ni- oder Co- based annealed 800 15 - 60 15 - 50 15 - 50 15 - 40 15 - 50 10 - 30 - 8 - 25 - - - S Ni- oder Co- based casting 1100 15 - 50 15 - 40 15 - 40 15 - 40 15 - 40 5 - 18 - 4 - 15 - - - Ni- oder Co- based hardened 1200 15 - 50 15 - 40 15 - 40 15 - 40 15 - 40 5 - 18 - 4 - 15 - - -Titanium alloys, high strengthPure titanium500 - 700100 - 21090 - 180-80 - 170-80 - 130-80 - 130---i Alpha- and beta-alloys, hardened 700 - 1000 40 - 90 40 - 80 - 40 - 70 - 20 - 40 - 15 - 35 - - - hardened and tempered 1000 - 1350 30 - 55 30 - 50 - 30 - 45 - - - - - - - Hardened steel H Hard cast iron hardened and tempered 1350 - 1700 15 - 25 10 - 25 - 15 - 25 - - - - - - -casting135040 - 8040 - 70-40 - 65------- Hardened cast iron hardened and tempered 1900 15 - 30 10 - 25 - 15 - 25 - - - - - - - The datas cutting speeds given are approximate values. More grades on the It is necessary to adjust them to the individual machining operation. following pages. ARNO®-Werkzeuge | Drehen | Turning | Точение 451