Заказ инструмента: http://steelcam.org | 8 (343) 382-52-03 | sales@sverla-ekb.ru 5230VS09 Recommended Speeds Speed vc (m/min) Wear Resistance 5230VS Series -- + Shoulder Mills Speed min. - max. Coolant Recommendation CVD PVD CVD Recommended  Possible  X Grade Standard Standard ISO Materials Rm and X500 SP6519 MP91M Hardness <600 N/mm2 130 - 270 130 - 295 140 - 345 Unalloyed <180 HBN      Steel <950 N/mm2 115 - 240 115 - 260 120 - 305 <280 HBN P 700-950 N/mm2 100 - 210 100 - 230 105 - 270 200-280 HBN      Alloyed 950-1200 N/mm2 75 - 160 75 - 175 80 - 205 Steel 280-355 HBN 1200-1400 N/mm2  50 - 100  50 - 110  50 - 130 355-415 HBN Austenitic + Ferritic 115 - 250 115 - 270 Stainless 300 series     M Steel Martensitic 100 - 220 105 - 235 400 series PH Stainless Refractory  50 - 110  50 - 120 P.H. Grey 120 - 280 140 - 295 145 - 365 GG-Ft K Cast Iron Spheroidal-Ductile   105 - 205   110 - 240  115 - 285 GGG-FGS Malleable 95 - 170 100 - 220 105 - 260 GTS - MN/MP Aluminium & Alloys N Aluminium < 16% Si 116 HBN & Alloys Aluminium + Silicon > 16% Si 92 HBN Iron Based 23 - 48 23 - 55 High Cobalt Based 21 - 44 22 - 48 S Temperature   Alloys Nickel Based 24 - 51 25 - 55 Titanium Based 35 - 73 36 - 79 Hard Steel >1400 N/mm2 H Hard >415 HBN Materials Chilled Cast Iron >1400 N/mm2 > 400 HBN www.kennametal.com A175