Скорость резания (1) Подача в зависимости от диаметра сверла, мм/об

Vc м/минVc м/минDR-05DR-06DR-07DR-09DR-12DR-16
IC908 внешнийIC9080 внешнийGF/DTGF/DTGF/DTGF/DTGF/DTGF/DT

200-300 260-390

0.06-0.100.07-0.120.08-0.120.10-0.150.12-0.160.14-0.17
0.10-0.150.10-0.160.12-0.180.14-0.220.15-0.250.16-0.26

150-200 190-260 150-220 190-290

0.06-0.100.07-0.120.08-0.120.10-0.140.12-0.150.14-0.16
120-180160-2300.10-0.140.10-0.150.10-0.160.14-0.200.14-0.220.15-0.24
120-190160-2500.06-0.100.06-0.100.06-0.100.08-0.120.10-0.150.14-0.17
100-160210-3100.10-0.140.10-0.140.10-0.140.12-0.180.14-0.200.16-0.24
160-240210-3100.06-0.100.06-0.100.06-0.120.08-0.120.10-0.140.12-0.20

150-250 190-320

0.10-0.22 0.10-0.22 0.10-0.22 0.15-0.25 0.18-0.30 0.20-0.34

120-180 160-230

150-300 190-390 0.12-0.25 0.12-0.25 0.12-0.25 0.20-0.30 0.2-0.35 0.28-0.45

20-50 30-60

50-60 60-80 20-50 30-60

0.04-0.080.04-0.080.05-0.090.07-0.100.08-0.120.10-0.14
0.05-0.080.05-0.080.06-0.090.07-0.100.08-0.120.10-0.14

(1) Сплав центральной пластины - всегда IC908.

  • Данные таблицы указаны для свёрл 2/3D. Для свёрл 4xD уменьшайте режимы на 15%.
  • При использовании только внешнего охлаждения снижайте подачу на 10%.
  • Используйте внутреннее охлаждение при обработке аустенитной нержавеющей стали.