| Tensile Strength | Hardness | Material | 0.25-1.00 | Lead( 1.25-1.50 | mm) 1.75-2.00 | 2.50-6.00 | ||
| ISO Material | Condition | [N/mm2] | HB | No. | Number o | fpasses | ||
| < 0.25 %C | Annealed | 420 | 125 | 1 | ||||
| >= 0.25 %C | Annealed | 650 | 190 | 2 | ||||
| Non-alloy steel and cast steel, < 0.55 %C | Quenched and tempered | 850 | 250 | 3 | ||||
| free cutting steel | Annealed | 750 | 220 | 4 | ||||
| >= 0.55 %C | Quenched and tempered | 1000 | 300 | 5 | ||||
| Annealed | 600 | 200 | 6 | |||||
| P Low alloy and cast steel (less | 930 | 275 | 7 | 1 | 1 | 2 | 3 | |
| than 5% of alloying elements) | Quenched and td | 1000 | 300 | 8 | ||||
| empere | 1200 | 350 | 9 | |||||
| Annealed | 680 | 200 | 10 | |||||
| High alloyed steel, cast steel and tool steel | Quenched and tempered | 1100 | 325 | 11 | ||||
| Stainless steel and cast steel | Ferritic/martensitic | 680 | 200 | 12 | ||||
| Martensitic | 820 | 240 | 13 | |||||
| M Stainless steel | Austenitic, duplex | 600 | 180 | 14 | 1 | 1 | 2 | 3 |
| Grey cast iron (GG) | Ferritic/pearlitic | 180 | 15 | |||||
| Pearlitic /martensitic | 260 | 16 | ||||||
| K Nodular cast iron (GGG) | Ferritic | 160 | 17 | 1 | 1 | 2 | 3 | |
| Pearlitic | 250 | 18 | ||||||
| Ferritic | 130 | 19 | ||||||
| Malleable cast iron | Pearlitic | 230 | 20 | |||||
| Aluminum- wrought alloy | Not hardenable Hardenable | 60 100 | 21 22 | |||||
| Not hardenable | 75 | 23 | 1 | 1 | 1 | 1 | ||
| Aluminum- | Hardenable | 90 | 24 | |||||
| cast, alloyed >12% Si | High temperature | 130 | 25 | 1 | 1 | 2 | 3 | |
| N >1% Pb | Free cutting | 110 | 26 | |||||
| Copper alloys | Brass | 90 | 27 | |||||
| Electrolytic copper | 100 | 28 | ||||||
| Non metallic | Duroplastics, fiber plastics | 29 | 1 | 1 | 1 | 1 | ||
| Hard rubber | 30 | |||||||
| Fe based | Annealed | 200 | 31 | |||||
| Hardened | 280 | 32 | ||||||
| High temperature alloys Ni C | Annealed | 250 | 33 | |||||
| S or o based | Hardened | 350 | 34 | 2 | 2 | 2 | 3 | |
| Cast | 320 | 35 | ||||||
| Pure | 400 | 36 | ||||||
| Titanium alloys | Alpha+ beta alloys, hardened | 1050 | 37 | |||||
| Hardened steel | Hardened | 55 HRC | 38 | |||||
| Hardened | 60 HRC | 39 | ||||||
| H Chilled cast iron | Cast | 400 | 40 | 3 | 3 | 3 | 3 | |
| Cast iron | Hardened | 55 HRC | 41 | 2 | 2 | 2 | 3 |
Rm - ultimate tensile strength, MPa