Recommended Cutting Data Turning – CERMET / PCD / CBN / HSS Cutting speed Vc [m/min] HSS-TiAlN ISO Material strength [N/mm2] AH7510 AH7516 AH7520 HSS-TiN AB8020 AP6010 AP6510 Tensile AC90C ACE6 T15 ca. 0,15% C 350 100 - 500 160 - 460 100 - 450 100 - 400 100 - 400 - - - - 70 - 100 80 - 110 Unalloyed steel and cast steel ca. 0,45% C 650 80 - 500 90 - 430 80 - 450 80 - 370 80 - 370 - - - - 65 - 90 70 - 100 ca. 0,75% C 1000 50 - 350 60 - 400 50 - 350 50 - 350 60 - 280 - - - - 35 - 55 30 - 60 600 80 - 500 90 - 350 80 - 450 80 - 300 80 - 300 - - - - 30 - 80 35 - 90 Low alloyed steel and cast steel 900 70 - 500 80 - 300 70 - 450 70 - 270 70 - 300 - - - - 30 - 80 35 - 90 P 1200 50 - 350 60 - 300 50 - 350 50 - 250 80 - 220 - - - - 30 - 60 35 - 70 High alloyed steel, high alloyed annealed 700 60 - 320 90 - 230 60 - 250 80 - 200 60 - 200 - - - - 30 - 60 35 - 70 tool steel and cast steel hardened and tempered 1100 50 - 180 60 - 180 50 - 180 50 - 160 60 - 200 - - - - - - ferritic / martensitic, annealed 700 80 - 350 90 - 290 80 - 300 80 - 250 70 - 270 - - - - 20 - 35 20 - 40 Stainless steel and cast steel martensitic, hardened and tempered 1000 80 - 400 - 80 - 350 80 - 250 70 - 250 - - - - - - austenitic and austenitic/ferritic 450 - 600 80 - 380 - 80 - 300 80 - 240 80 - 240 - - - - 20 - 35 20 - 40 M Stainless steel and cast steel chilled 600 - 900 60 - 350 - 60 - 300 80 - 240 80 - 200 - - - - - - pearlitic, ferritic 500 - 700 100 - 500 - 100 - 300 80 - 300 - 700 - 2000 - - - - - Cast iron pearlitic, martensitic 700 - 850 100 - 380 - 100 - 300 80 - 260 - 500 - 900 - - - - - 800 - 1100 100 - 350 - 100 - 300 80 - 240 - - - - - - - K Cast iron with nodular graphite ferritic 550 80 - 350 80 - 300 100 - 300 80 - 300 80 - 300 - - - - - - pearlitic 800 80 - 350 80 - 250 100 - 300 80 - 250 80 - 250 - - - - - - ferritic 450 80 - 350 80 - 350 100 - 300 80 - 350 80 - 350 - - - - - - Malleable cast iron pearlitic 750 80 - 350 60 - 250 100 - 300 60 - 250 60 - 250 - - - - - - not heat treatable 200 - - - - - - - - 400 - 2500 400 - 900 400 - 900 Aluminum alloys, long chipping heat treatable, heat treated 350 - - - - - - - - 300 - 2500 140 - 240 150 - 250 ≤ 12% Si, hardened 250 - - - - - - - - 400 - 2000 140 - 240 150 - 250 Casted aluminum alloys ≤ 12% Si, heat treatable, heat treated 300 - - - - - - - - 400 - 2000 140 - 240 150 - 250 ≤ 12% Si, not heat treatable 450 - - - - - - - - 400 - 1800 60 - 130 70 - 140 Lead alloys, Pb > 1% 400 - - - - - - - - 300 - 1800 90 - 110 100 - 120 N Copper and copper alloys Brass, bronze 300 - - - - - - - - 400 - 1600 - - (brass / bronze) Aluminum bronze 500 - - - - - - - - 300 - 1800 - - Copper and electrolyte copper 200 - - - - - - - - 300 - 1800 110 - 180 120 - 200 Duroplastics - - - - - - - - - 80 - 140 90 - 150 Non-ferrous materials Reinforced plastics - - - - - - - - 200 - 900 - - Hard rubber - - - - - - - - - - - Fe-alloyed annealed 700 - - - - - 300 - 500 - - - 10 - 20 10 - 25 Fe-alloyed hardened 950 - - - - - 250 - 350 - - - 10 - 20 10 - 25 High temperature resistant alloys Ni- oder Co- based annealed 800 - - - - - 280 - 400 - - - 10 - 20 10 - 25 S Ni- oder Co- based casting 1100 - - - - - 200 - 300 - - - - - Ni- oder Co- based hardened 1200 - - - - - 200 - 300 - - - - - i Titanium alloys, high strength Alpha- and beta-alloys, hardened Pure titanium hardened and tempered 500 - 700 700 - 1000 1000 - 1350 - - - - - - - - - - - - - - - - - - - - 120 - 250 - - 80 - 180 100 - 400 100 - 350 - 15 - 30 15 - 30 - 15 - 35 15 - 35 - Hardened steel hardened and tempered 1350 - 1700 - - - - - - - 50 - 150 - - - H Hard cast iron casting 1350 - - - - - 60 - 150 - - - - - Hardened cast iron hardened and tempered 1900 - - - - - 50 - 150 - - - - - The datas cutting speeds given are approximate values. More grades on the It is necessary to adjust them to the individual machining operation. following pages. 456 ARNO®-Werkzeuge | Drehen | Turning | Точение